Title: SP-123: Design of Beam-Column Joints for Seismic Resistance

Author(s): Editor: James O. Jirsa

Publication: Special Publication

Volume: 123

Issue:

Appears on pages(s): 514

Keywords:

Date: 1/1/1991

Abstract:
SP123 This volume is a collection of technical papers on the aspects of design of beam-column joints for seismic resistance. Nineteen papers are divided into the following groups. - Tests conducted on specimens designed using current codes but with the same general geometry and a specified loading history. (4 papers) - Design recommendations -- Japan. (1 paper) - Influence of joint geometry on strength and deformation characteristics. (8 papers) - Influence of bond on joint performance. (4 papers) - Joint in precast systems and with high-strength materials. (2 papers)