Title: SP-109: Concrete in Marine Environment

Author(s): Editor: V.M. Malhotra

Publication: Symposium Paper

Volume: 109

Issue:

Appears on pages(s): 748

Keywords:

Date: 8/1/1988

Abstract:
SP109 The book offers information on a variety of subjects such as: The durability of concrete containing supplementary cementing materials; the durability and corrosion of reinforced concrete subjected to a marine environment; and the repair, design and construction of concrete structures in a marine environment. Whether you are building a new concrete structure in marine environment, or repairing an old one--as an engineer you need the wealth of information contained within the 32 papers presented in this important symposium volume.




  

Please enter this 5 digit unlock code on the web page.