ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: SP-074: Monolithic Refractories

Author(s): Editor: David R. Lankard / Sponsored by: ACI Committee 547

Publication: Symposium Paper

Volume: 74

Issue:

Appears on pages(s): 168

Keywords:

Date: 8/1/1982

Abstract:
Proceedings of the second ACI sponsored Refractory Concrete Symposium. Ten papers are presented. Topics include recent advances in refractory concrete technology; problems and solutions in using these materials as liners in coal gasification equipment, aluminum melting and holding, refining and petrochemical operations, and steelmaking; nondestructive testing and evaluation; and repair techniques. Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP74




  

Please enter this 5 digit unlock code on the web page.