Title: SP-008: Symposium on Concrete Construction in Aqueous Environment
Author(s): Ivan L. Tyler, Ben C. Gerwick Jr., George B. Wallace, J.W. Trahern, Morris Schupack, Winfred T. Robertson, Thane E. Brown, Wheeler H. Rucker Jr., C.C. Nichols, and H. Morgan Noble
Publication: Symposium Paper
Volume: 8
Issue:
Appears on pages(s): 116
Keywords:
Date: 1/1/1964
Abstract:
SP8
A collection of 10 papers on various aspects of the construction of concrete waterfront structures, concrete waterholding structures, and concrete construction in aqueous environments, Covers tremie concrete, prestressed tanks, concrete piles, joints and cracks, concrete pontoons, effect of sea water, and pier design.