Title: SP-210: Deflection Control for The Future
Author(s): Editor: NJ Gardner
Publication: Symposium Paper
Volume: 210
Issue:
Appears on pages(s): 250
Keywords:
Date: 2/1/2003
Abstract:
SP-210
This Symposium Publication contains papers presented during the 2002 ACI Spring Convention in Detroit, including six papers related to predicting the deflections of concrete members reinforced with fiber-reinforced polymer (FRP) reinforcement: one paper describes two field investigations, two unique laboratory investigations, a paper on estimating the errors in calculating deflections of high-performance concrete slabs, and a comparison of the ACI and EC2 deflection provisions. This volume should be read in association with Symposium Publication SP-203, Code Provisions for Deflection Control in Concrete.