Title: SP-207: Proceedings, 3rd Intl Conf on High Performance Concrete: Performance and Quality of Concrete Struct
Author(s): Editors: V.M. Malhotra, Paulo Helene, Enio P. Figuerido, and Armando Carniero
Publication: Symposium Paper
Volume: 207
Issue:
Appears on pages(s): 514
Keywords:
Date: 10/7/2002
Abstract:
This Symposium Publication includes 30 papers selected from the Third Conference on High-Performance Concrete (HPC) and Performance and Quality of Concrete Structures, held in Brazil. Topics covered include chloride penetration models in reinforced concrete structures, high-strength concrete with crushed and natural sand, sewage sludge ash as an addition in concrete, and the mechanical properties of polymer-modified high-performance lighweight aggregate concrete.
Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order.