Short-Term Impact of High-Aggregate Fines Content on Concrete Incorporating Water-Reducing Admixtures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Short-Term Impact of High-Aggregate Fines Content on Concrete Incorporating Water-Reducing Admixtures

Author(s): Mohamed Nagib Abou-Zeid and Maged Maher Fakhry

Publication: Materials Journal

Volume: 100

Issue: 4

Appears on pages(s): 280-285

Keywords: concrete; fine aggregate; mixture proportion; water-reducing admixture.

DOI: 10.14359/12665

Date: 7/1/2003

Abstract:
Water-reducing and high-range water-reducing admixtures have been increasingly involved in concrete works. Aggregate fines passing sieve No. 200 (75 mm) are produced in large quantities; and, recently, some efforts have been exerted to investigate the feasibility of using such fines in concrete. The interaction between water-reducing admixtures and aggregate fines, however, has been questioned and is not fully understood yet. This paper represents a major part of a larger scale study addressing aggregate fines smaller than 75 mm used with a wide range of constituent materials and proportions. This paper covers 19 mixtures that were prepared with dolomite coarse aggregates, with and without fines, and with water-reducing and high-range water-reducing admixtures. Results indicate that the fines tested differed significantly from their parent rocks in physical and chemical properties. High fines also resulted in a remarkable increase in water demand, poor slump, and high slump loss. High admixture dosages fail in enhancing concrete workability/consistency in the presence of high fines content unless the water-cement ratio (w/c) is increased. At the same w/c, the fines contributed to some increase in compressive strength and improvement in flexural strength.