Title: First Slip-Formed Apartment Building in the United States

Author(s): John H. Doggett

Publication: Journal Proceedings

Volume: 54

Issue: 3

Appears on pages(s): 767-772

Keywords: no keywords

Date: 3/1/1958

Abstract:
Upper eight stories ol ten-story apartment building wcrc slip formed in 115 hr of around-the-clock operations. Structural framing, building of the forms, and construction practices are described, citing advantages peculiar to the method.




  