Title: Wear-Resistant Concrete Construction

Author(s): Shu-T’ien Li

Publication: Journal Proceedings

Volume: 55

Issue: 2

Appears on pages(s): 879-892

Keywords: no keywords

Date: 2/1/1959

Abstract:
Presents requirements for materials, methods, and workmanship in constructing or resurfacing floors, platforms, and aprons subject to heavy traffic or to severe use from the handling of heavy materials. Various methods of treating wearing surfaces made of concrete are discussed.