Title: Design of Unreinforced Slabs on Ground Made Easy

Author(s): Wayne Walker and Jerry Holland

Publication: Concrete International

Volume: 23

Issue: 5

Appears on pages(s): 37-42

Keywords:

DOI:

Date: 5/1/2001

Abstract:
In our previous article The First Commandment for Floor Slabs: Thou Shalt Not Curl Nor Crack...(Hopefully) (Concrete International, January 1999), we discussed some important concepts concerning the design of slabs-on-ground such as curling, linear shrinkage, joint spacing, and serviceability issues. Using these concepts we have developed design aids for slabs-on-ground that are unreinforced or have a small amount of reinforcing that is not included in the structural capacity, which are covered in this article. We have used these design aids for many years to design numerous high quality industrial slabs. Design graphs presented here for joint spacings, uniform loads, rack loads, and lift truck loads help make the design of unreinforced slabs much simpler and easier; furthermore, these design aids usually provide more economical slabs than those designed by more traditional methods.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer