Title: Shear Database for Prestressed Concrete Members

Author(s): Eisuke Nakamura, Alejandro R. Avendaño, and Oguzhan Bayrak

Publication: Structural Journal

Volume: 110

Issue: 6

Appears on pages(s): 909-918

Keywords: prestressed concrete; shear database; shear design procedure; shear strength

DOI: 10.14359/51686147

Date: 11/1/2013

Abstract:
The University of Texas Prestressed Concrete Shear Database (UTPCSDB) was developed and expanded to include 1696 tests reported in North America, Japan, and Europe from 1954 to 2010. The UTPCSDB was subsequently used to examine the accuracy and conservativeness of shear design procedures based on different rationales. The results of the examination revealed that design expressions based on the Modified Compression Field Theory (MCFT) yielded the most accurate shear strength estimations for prestressed concrete members that failed in typical shear failure modes. Most of the unconservative estimations that resulted from the use of the MCFT-based design expressions were observed in specimens that failed in shear but exhibited signs of horizontal shear damage or anchorage zone distress. Although the ACI 318-11 detailed method provided slightly less-conservative estimations than the MCFT-based design expressions, these estimations were more accurate than those obtained by using other empirical shear design equations.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer