Abstract:

Ultra-high-performance concrete (UHPC) is an advanced cementitious composite material with extraordinary mechanical and durability properties. This article discusses the construction of a short-span bridge using UHPC as well as the cost considerations associated with building an entire bridge with UHPC and reflects on lessons learned from the process.


Document: 

SP364_2

Date: 

December 1, 2024

Author(s):

Youjin Chae, Min-Jun Jeon, Chang-Kil Ju, Seung-Il Kim, and Tae-Sung Eom

Publication:

Symposium Papers

Volume:

364

Abstract:

Modular construction has been attracting attention worldwide as a promising solution to reduce construction time and labor demand. In this study, a new inter-module composite floor system that connects the upper module floor beams and lower module ceiling beams was experimentally and analytically investigated with an emphasis on vibration performance under service loading. First, the upper module floor of 2 m [6.56 ft] wide and 6 m [19.7 ft] long was fabricated as a composite system consisting of precast concrete (PC) panels, steel beams and ultra high-performance concrete (UHPC) connectors. Structural integrity between PC panels, steel beams and UHPC connectors were secured using grouting and topping mortar. Then, the lower module ceiling beams were connected to the upper module floor beams by fully tensioned high-tension bolts (i.e., slip-critical connection) to complete the inter-module composite floor. The vibration frequencies, damping ratio, and acceleration responses of the inter-module composite floors were measured from laboratory tests such as impact hammer, heel drop and walking tests, considering the number and location of the connecting bolts as the test parameter. The vibration characteristics of the inter-module composite floors were investigated further through finite element analysis. The measured and predicted vibration performances were compared with the acceptance criteria in AISC Design Guide 11 and ISO 10137.

DOI:

10.14359/51745454


Document: 

SP363

Date: 

July 25, 2024

Author(s):

ACI Committee 345

Publication:

Symposium Papers

Volume:

363

Abstract:

Ultra-high performance concrete (UHPC) is a state-of-the-art cementitious composite. Since the concept of this novel concrete mixture emerged in the 1990s, significant advancements have been made with numerous benefits such as high strength, flowability, high post-cracking tensile resistance, improved durability, reduced maintenance, and extended longevity. Currently, UHPC is employed around the globe alongside recently published practice guidelines. Although numerous research projects were undertaken to examine the behavior of UHPC-incorporated structures, there still are many gaps to be explored. Of interest are the development of robust and reliable mixtures and their application to primary load-bearing members for bridges and buildings, including various site demonstration projects that would promote the use of this leading-edge construction material. This Special Publication (SP) contains nine papers selected from three technical sessions held in the ACI Spring Convention in March 2022. All manuscripts were reviewed by at least two experts in accordance with the ACI publication policy. The Editors wish to thank all contributing authors and anonymous reviewers for their rigorous efforts. The Editors also gratefully acknowledge Ms. Barbara Coleman at ACI for her knowledgeable guidance. Yail J. Kim, Steven Nolan, and Antonio Nanni Editors University of Colorado Denver Florida Department of Transportation University of Miami

DOI:

10.14359/51742116


Document: 

SP-363-2

Date: 

July 1, 2024

Author(s):

Daniel J. Alabi, Megan S. Voss, Raid S. Alrashidi, Christopher C. Ferraro, Kyle Riding, and Joel B. Harley

Publication:

Symposium Papers

Volume:

363

Abstract:

Ultra-high performance concrete (UHPC) has seen growing use in the construction industry because of its high compressive, tensile, and flexural strength. The tensile and flexural strength are in part due to the steel fibers added to the UHPC mix. Yet, fibers can segregate due to poor material rheological properties and construction practices, resulting in less than expected material strength. Due to the importance of these fibers, there is a need to verify the volume and orientation of the steel fibers in the UHPC. In this work, we report on the design and testing of electromagnetic sensor systems that are able to test the integrity of the steel fibers in the UHPC structure. We test our sensor system using UHPC samples containing 1% to 3% fiber content by volume and created a calibration based on the results. Our results show a linear relationship between the inductance change versus the fiber percentage with an R-squared value of 99.7 %, which shows that our approach successfully demonstrated the potential of using our approach for characterizing steel fibers in UHPCs.

DOI:

10.14359/51742105


Document: 

SP-363-7

Date: 

July 1, 2024

Author(s):

Kusum Saini and Vasant A. Matsagar

Publication:

Symposium Papers

Volume:

363

Abstract:

Lightweight and high-performance materials have become necessary for infrastructure with advanced construction and performance requirements. One of the major challenges with structures made of these materials is their performance under natural and man-made hazards, such as wind, fire, and blast. Therefore, in this study, the performance of ultra-high-performance concrete (UHPC) and UHPC coated with foamed concrete (UHPC-Foamed) and polyurea (UHPC-Polyurea) is investigated under blast load. A finite element model is developed to assess the behavior of UHPC and coated UHPC panels under far-field and near-field blast scenarios. The constitutive behaviors of UHPC and foamed concrete are considered using the concrete damage plasticity model with respective parameters. The polyurea is modeled as a hyperelastic material with the Mooney-Rivlin model. Moreover, the effectiveness of the additional coatings, i.e., foamed concrete and polyurea, on the blast resistance of each panel is presented. The finding of the study shows that both foamed concrete and polyurea enhance the blast resistance of the UHPC concrete panels. Moreover, a comparison between the blast resistance of UHPC-Foamed and UHPC-Polyurea is conducted under far-field and near-field blast scenarios. Also, the effectiveness of foamed concrete and polyurea coatings with different thicknesses to UHPC panels is assessed under both blast scenarios.

DOI:

10.14359/51742110


12345...>>

Results Per Page 





ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer