International Concrete Abstracts Portal

Showing 1-5 of 1039 Abstracts search results

Document: 

SP365_10

Date: 

March 1, 2025

Author(s):

Anca Ferche and Vahid Sadeghian

Publication:

Symposium Papers

Volume:

365

Abstract:

Developed 40 years ago by Frank Vecchio and Michael Collins, the Modified Compression Field Theory (MCFT) and its successor, the Disturbed Stress Field Model (DSFM), have proven to be robust methodologies in modeling the response of concrete structures. Originally developed for newly designed concrete structures, they have been refined over the years to expand their applicability to various engineering problems, including modeling deteriorated and repaired structures. This paper reviews the evolution and application of MCFT in modeling and assessment of deteriorated and repaired concrete structures. The first part focuses on the application of MCFT to advanced field structural assessment, including stochastic analysis procedures that incorporate field data. The second part discusses the evolvement of MCFT to account for two of the most common deterioration mechanisms, reinforcement corrosion and alkali-silica reaction. The last part explores the application of the model to structures repaired with fiber-reinforced polymer composites. It is concluded that the extension of the MCFT formulation has enabled it to reliably predict the behavior of both deteriorated and repaired concrete structures.

DOI:

10.14359/51746690


Document: 

SP364_4

Date: 

December 1, 2024

Author(s):

Mohammad T. Nikoukalam, Shahabeddin Torabian, and Said Bolourchi

Publication:

Symposium Papers

Volume:

364

Abstract:

This research examines the hole-drilling method per ASTM E837, known for its minimal invasiveness, for measuring in situ stress in reinforcing bars embedded within concrete structures. The primary objective is to ascertain the applicability of this method in estimating non-apparent stresses, such as those resulting from the external loads, creep, shrinkage, or alkali-silica reaction, that are needed for structural assessment. Systematic experiments on reinforced concrete beams are conducted to validate the method’s viability in identifying these critical in situ stresses. The findings highlight the potential of the hole-drilling method to enhance structural health monitoring practices, offering an accurate tool for assessing stress states crucial for the maintenance and safety of concrete structures. The results demonstrated that while the hole-drilling method is robust for moderate-stress evaluations (up to about 70% of the nominal yield stress), it overestimates the stress in the reinforcing bar under high-stress conditions near the 100% nominal yield stress. This study contributes to the field by confirming the limits and applicability of the ASTM E837 standard for estimating the existing stress in the embedded reinforcing bars.

DOI:

10.14359/51745456


Document: 

SP362

Date: 

June 30, 2024

Author(s):

ACI, RILEM, Université de Sherbrooke, Université Toulouse III, CRIB, LMDC Toulouse

Publication:

Symposium Papers

Volume:

362

Abstract:

In July of 1983, the Canada Centre for Mineral and Energy Technology of Natural Resources Canada (CANMET), in association with the American Concrete Institute (ACI) and the U.S. Army Corps of Engineers, sponsored a 5-day international conference in Montebello, Quebec, Canada, on the use of fly ash, silica fume, slag, and other mineral by-products in concrete. The conference brought together representatives from industry, academia, and government agencies to present the latest information on these materials and to explore new areas of needed research. Since then, eight other such conferences have been held around the world (Madrid, Trondheim, Istanbul, Milwaukee, Bangkok, Madras, Las Vegas, and Warsaw). The 2007 Warsaw Conference was the last in this series. In 2017, due to the renewed interest in alternative and sustainable binders and supplementary cementitious materials, a new series was launched by Sherbrooke University (Professor Arezki Tagnit-Hamou), American Concrete Institute (ACI), and the International Union of Laboratories and Experts in Construction Materials, Systems and Structures (RILEM)—in association with a number of other organizations in Canada, the United States, and the Caribbean—sponsored the 10th ACI/RILEM International Conference on Cementitious Materials and Alternative Binders for Sustainable Concrete (ICCM2017). The conference was held October 2-4, 2017, in Montréal, Canada. The conference proceedings, containing 50 reviewed papers from more than 33 countries, were published as ACI SP-320. In 2021, UdeS, ACI, and RILEM, in association with Université de Toulouse and a number of other organizations in Canada, the United States, and Europe, sponsored the 11th ACI/RILEM International Conference on Cementitious Materials and Alternative Binders for Sustainable Concrete (ICCM2021). The conference was scheduled to take place in Toulouse, but due to COVID, it was held online June 7-10, 2021. The conference proceedings, containing 53 reviewed papers from more than 21 countries, were published as ACI SP-349. In 2024, the conference was finally held in-person in Toulouse from June 23 to 26, 2024, with the support of UdeS, ACI, and RILEM in association with Université de Toulouse (Martin Cyr) and a number of other organizations in Canada, the United States, and Europe. The purpose of this international conference was to present the latest scientific and technical information in the field of supplementary cementitious materials and novel binders for use in concrete. The new aspect of this conference is to highlight advances in the field of alternative and sustainable binders and supplementary cementitious materials for the transition to low carbon concrete. The conference proceedings, containing 78 reviewed papers from more than 25 countries, have been published as ACI SP-362. Thanks are extended to the members of the International Scientific Committee who reviewed the papers. The cooperation of the authors in accepting the reviewers’ suggestions and revising their manuscripts accordingly is greatly appreciated. The involvement of the steering committee and the organizing committee is gratefully acknowledged. Special thanks go to Chantal Brien (Université de Sherbrooke) for the administrative work associated with the conference and for processing the manuscripts for both the ACI proceedings and the supplementary volume. Arezki Tagnit Hamou, Editor Chairman, 12th ACI/RILEM International Conference on Cementitious Materials and Alternative Binders for Sustainable Concrete (ICCM2024). Sherbrooke, Canada, 2024

DOI:

10.14359/51742032


Document: 

SP-362_76

Date: 

June 18, 2024

Author(s):

Wena de Nazaré do Rosario Martel, Josée Duchesne, and Benoît Fournier

Publication:

Symposium Papers

Volume:

362

Abstract:

Due to its predominant soda-lime composition, most post-consumer glass processed by recycling facilities would be classified as high-alkali pozzolanic glass powder (GP). In cementitious matrices, the intrinsic alkaline pore solution induces the dissolution of both silica and alkali ions. Therefore, the GP can potentially induce two similar reactions in concrete: either a deleterious alkali-silica reaction or a pozzolanic reaction. The equilibrium of the pore solution will determine which reaction will prevail in the long term. To understand the chemical stability of GP in a cementitious system, the evolution of the solubility of key elements in an alkali-rich synthetic pore solution was studied as a function of reaction time, particle size, presence of Ca(OH)2 and CaCO3, and binder/solution ratio (B/S). The solution was based on the R³ method, which consists mainly of lab-grade chemicals such as KOH and K2SO4. Although the chemical equilibrium seems to be fully reached in the first hours of hydration, the main products, such as C-S-H, are unstable because the alkali leaching/uptake in the C-S-H chains is dynamically evolving. The experiments show that both C-S-H precipitation and alkali leaching rates increase with increasing B/S ratio and decreasing particle size, and are directly related to the presence of calcium in the solution.

DOI:

10.14359/51742026


Document: 

SP-362_65

Date: 

June 18, 2024

Author(s):

Kwangwoo Wi, Oguzhan Sahin, Kejin Wang, Yunsu Lee

Publication:

Symposium Papers

Volume:

362

Abstract:

The management of municipal solid waste incineration fly ash (MSWI FA) has become a critical issue as its generation increases rapidly along with the global population growth. In this study, MSWI FA was treated via water-washing, and then the untreated and water-treated MSWI FAs (RFA and WFA) were blended with mainstream supplementary cementitious materials (SCMs), including ground granulated blast-furnace slag (GS), silica fume (SF), and limestone powder (LS). The MSWI FASCMblends were used as a cement replacement in a mortar. The content of MSWI FAs was set at 10% (by weight of binder) for all mortar mixtures. The content of GS and LS was also set at 10%, while the SF content was 2.5%. Flowability, setting time, isothermal calorimetry, compressive strength, and free-drying shrinkage tests were performed. The results showed that mortars containing raw (untreated) fly ash (RFA) had reduced strength, whereas mortars containing water-treated fly ash (WFA) displayed comparable or even higher strength than the control mortar (made with 100% cement) after 28 days. While mortars containing RFA showed increased drying shrinkage, mortars containing WFA exhibited diminutive or no increase in drying shrinkage when compared to the control mortar. Based on the test results, the mixture with a cement:WFA:GS ratio of 80:10:10 was the optimal binder for concrete applications.

DOI:

10.14359/51742015


12345...>>

Results Per Page 





ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.