International Concrete Abstracts Portal

Showing 1-5 of 246 Abstracts search results

Document: 

SP-362_16

Date: 

June 5, 2024

Author(s):

Torben Gädt, Simon Nickl

Publication:

Symposium Papers

Volume:

362

Abstract:

Calcined clays are a very promising supplementary cementitious material. A remaining challenge for a widespread application is the rheology of calcined clay containing cementitious materials. The water and superplasticizer demand and the viscosity of calcined clay binders are higher than for normal Portland cement (PC) binders. Consequently, there is a need to improve the understanding of the rheological properties of calcined clay-based binders. Here, we report on the rheological characteristics of four polycarboxylate ether superplasticizers in Portland cement and LC3 pastes. The superplasticizer chemistry is controlled through polymer synthesis. We chose simple slump flow tests to characterize the rheology of the pastes at different superplasticizer dosages. Furthermore, we characterize the initial reactivity of the binder using in-situ calorimetry. All four polymers exhibit very similar properties in the LC3 system, while the differences are much more prominent in Portland cement. The dosage efficiency in the LC3 system is lower for all polymers, and the most dosage-efficient superplasticizer in the LC3 system is only ranked third in Portland cement. Finally, the very early heat flow of the suspensions indicates that dissolution and early hydrate phase formation of the PC are promoted in LC3 systems. We propose that the increased PC reactivity is partly responsible for the larger slump loss of LC3 binders.

DOI:

10.14359/51740886


Document: 

SP354

Date: 

July 1, 2022

Author(s):

Sponsored by: ACI Committees 212, 236, 238, and 239

Publication:

Symposium Papers

Volume:

354

Abstract:

In May 1978, the Canada Centre for Mineral and Energy Technology (CANMET), in association with the American Concrete Institute (ACI) sponsored a 3-day conference in Ottawa, ON, Canada, on the use of superplasticizers in concrete. Selected papers from the conference were published as ACI SP-62. In 1981, CANMET, again in association with ACI, sponsored a second 3-day international conference in Ottawa on the use of the superplasticizers in concrete. Proceedings of the conference were published as ACI SP-68. The purpose of the third international conference in Ottawa in 1989 was to review the progress made since the meetings in 1978 and 1981, and to bring together representatives of the chemical admixtures, cement, and concrete industries to exchange information and delineate new areas of needed research. The scope of this conference was expanded to include chemical admixtures other than superplasticizers. Proceedings of the conference were published as ACI SP-119. In October 1994, CANMET in association with ACI and several other organizations sponsored the fourth conference in Montreal, QC, Canada. The objective of this conference was to bring attention to new developments in chemical admixture since the last conference in 1989. The proceedings of the conference were published as ACI SP-148. In October 1997, the Committee for the Organization of CANMET/ACI International Conference, (ACI Council), in association with ACI and several cement and concrete organizations in Italy, sponsored the fifth conference in Rome, Italy. The conference was aimed at transferring technology in the fast-moving field of chemical admixtures. The proceedings of the conference were published as ACI SP-173. In October 2000, Committee for the Organization of CANMET/ACI International Conferences, (ACI Council), in association with several organizations in Canada and France, sponsored the sixth conference in Nice, France. More than 50 papers from more than 20 countries were received and reviewed by an ACI review panel, and 37 were accepted for publication in the proceedings of the conference. The proceedings were published as ACI SP-195. In October 2003, the Committee for the Organization of CANMET/ACI International Conferences (ACI Council) in association with several organizations in Canada and Germany, sponsored the seventh conference in Berlin, Germany. The conference attracted more than 275 delegates and proceedings of the conference consisting of 39 papers, were published as ACI SP-217. In October 2006, the Committee for the Organization of CANMET/ACI International Conferences, (ACI Council), sponsored the eighth conference in Sorrento, Italy. More than 60 papers from more than 25 countries were received, and peer reviewed by the CANMET/ACI review panel in Budapest, and 36 were accepted for publication as ACI SP-239. In October 2009, the Committee for the Organization of International Conferences (COIC) (formerly CANMET/ACI International Conferences) sponsored the ninth ACI International Conference in Seville, Spain. More than 50 papers from more than 20 countries were received and peer reviewed, and 35 were accepted for publication in the proceedings of the conference. The proceedings were published as ACI SP-262. In October 2012, COIC sponsored the Tenth International Conference on Superplasticizers and Other Chemical Admixtures in Concrete in Prague, Czech Republic. More than 70 papers from all over the world were peer reviewed, and 33 were accepted for publication in the proceedings of the conference. The proceedings were published as ACI SP-288. In July, 2015, the COIC in association with ACI sponsored the Eleventh International Conference on Superplasticizers and Other Chemical Admixtures in concrete in Ottawa, ON, Canada. More than 60 papers from the world over were peer reviewed, and 28 were accepted for publication in the proceedings of the conference. Also, additional papers were presented at the conference that were published in the Supplementary Papers Volume. In October 2018, the Chinese Ceramic Society and the China Academy of Building Research (CABR), Beijing China, in association with ACI, sponsored the Twelfth International Conference on Superplasticizers and other Chemical Admixtures in Concrete in Beijing China. More than 80 papers from all over the world were received and peer reviewed. A total of 36 refereed papers were accepted for publication in the proceedings of the conference. The proceedings were published by as ACI SP-329. The proceedings were published as ACI SP-302. Also, 54 additional papers were presented at the conference, and were published in the Supplementary Papers Volume. In July, 2022, after a postponement for the COVID-19 pandemic, the ACI Italy Chapter and the University of Bergamo, Italy, sponsored the Thirteenth International Conference on Superplasticizers and Other Chemical Admixtures in Concrete in Milan, Italy. The proceedings of the conference consisting of 35 refereed papers were published by ACI as SP-354. In addition to the refereed papers, about 20 other papers were presented at the conference, and were published in a supplementary papers volume. The main topics of the papers presented at the conference are related to superplasticizers, accelerating admixtures, retarding admixtures, air-entraining agents, shrinkage-reducing agents, superabsorbent polymers, and self-healing admixtures, and their influence on the properties of the concrete in fresh and hardened state. These properties include: workability, slump-loss, time of setting, heat of hydration, strength, durability, shrinkage, and creep of the concrete mixtures. Thanks are extended to the reviewers for the valuable efforts in reviewing all the manuscripts published in the conference proceedings and in the supplementary volume. The guidance from Dr. V. M. Malhotra and Prof. M. Collepardi, the Honorary Chairpersons of the conference, is sincerely appreciated. Also, acknowledged is the support of ACI International for the publication of the proceedings (ACI SP-354). The Editors Dr. Denny Coffetti Prof. Luigi Coppola Dr. Terence Holland

DOI:

10.14359/51736102


Document: 

SP-355_15

Date: 

July 1, 2022

Author(s):

Johann Plank, Lei Lei

Publication:

Symposium Papers

Volume:

355

Abstract:

Polycarboxylates (PCEs) currently dominate the global superplasticizer market. Among them, HPEG and IPEG PCEs have attained a prominent position as they present the most cost-effective PCEs known at present. Recently, novel vinyl ether PCEs designated as EPEG and GPEG PCEs were introduced, thus broadening the family of VPEG PCEs, and their overall performance is still evaluated. Well documented are now the advantages of novel phosphated comb polymers which can significantly reduce the stickiness of concrete e.g. in UHPC. In spite of many attempts, so far no overall cost-effective clay tolerant superplasticizer has been identified, the challenge being that such a structure must include side chains that however do not contain polyethylene glycol/polypropylene glycol (PEG/PPG) or polyamines. Fortunately, for calcined clay blended cements, HPEG PCEs of specific molecular design as well as zwitterionic (amphoteric) PCEs have proven to be highly effective. Moreover, AAS binder systems were successfully fluidized with APEG or HPEG PCEs exhibiting particularly short side chains (nEO < 10). This review underlines the critical role that innovation in chemical admixtures will play in the future to facilitate a successful migration to low-carbon binders.

DOI:

10.14359/51736021


Document: 

SP-355_28

Date: 

July 1, 2022

Author(s):

Charles Nmai, Chris Eagon, John Luciano

Publication:

Symposium Papers

Volume:

355

Abstract:

In the late 1980s, an innovative hydration-stabilizing admixture was introduced to help concrete producers effectively extend the working time of fresh concrete mixtures for challenging applications, particularly, in hot weather or long time-to-discharge applications. The hydration-stabilizing admixture also provided concrete producers with a means of managing returned concrete to address environmental issues associated with concrete waste. In recent years, admixtures that allow concrete producers to convert returned concrete into a very low-strength granular material that can be used for construction backfill, road base, or in other applications have been introduced. Together with the hydration-stabilizing admixture, concrete producers can now use chemical admixtures to significantly reduce concrete waste. In this paper, the operational and sustainability benefits of the hydration-stabilizing admixture and a new one-component engineered polymer admixture that facilitates the beneficial reuse of returned fresh concrete are presented and discussed.

DOI:

10.14359/51736040


Document: 

SP-354_07

Date: 

July 1, 2022

Author(s):

Wolfram Schmidt

Publication:

Symposium Papers

Volume:

354

Abstract:

Due to the high carbon dioxide emissions linked to concrete production and a rapidly increasing demand for cementitious materials, particularly in the global South, it is inevitable to use cement in concrete more efficiently. This requires chemical admixtures to enhance the overall performance of the binder and to cope with the negative rheological influences of supplementary cementitious materials that are used to replace ordinary Portland cement. However, particularly in the growing economies of the Southern hemisphere, where a massive part of the future construction activities will take place, the supply chains for performance-enhancing chemical admixtures are often poor, and local production facilities are lacking today. This paper presents case studies of polysaccharide-based alternative admixtures such as acacia gum, cassava starch, and the gum of the bark of Triumfetta pendrata A. Rich, which can be used effectively as superplasticizer, robustness enhancer, and thixotropy incorporating agent, respectively. Their modes of operation are discussed based on their spread flow, zeta potentials, and hydrodynamic diameters in the presence and absence of calcium ions.

DOI:

10.14359/51736063


12345...>>

Results Per Page 





ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.