Showing 1-5 of 283 Abstracts search results
Document:
24-071
Date:
January 1, 2025
Author(s):
Anthony Addai Boateng, Garrett Tatum, and Natassia Brenkus
Publication:
Materials Journal
Volume:
122
Issue:
1
Abstract:
Pourbacks and overlays are commonly used in bridge elements and repairs, as it is crucial to corrosion protection that the bond between grout and concrete in these regions is carefully constructed. The integrity of the bond is crucial to ensure a barrier against water, chloride ions, moisture, and contaminants; bond failure can compromise the durability of concrete structures’ long-term performance. This study examines the influence of surface preparation methods on the bond durability and chloride permeability between concrete substrate and grouts, including both non-shrink cementitious and epoxy grouts. A microstructural analysis of scanning electron microscopic (SEM) images was conducted to characterize the porosity of specimen interfaces. Pulloff testing was performed to quantify tensile strength. Results show that a water-blasted surface preparation technique improved the tensile bond strength for cementitious grout interfaces and reduced porosity at the interface. In contrast, epoxy grout interfaces were less affected by surface preparation. The study establishes a relationship between chloride ion permeability, porosity, and bond strength. The findings highlight the importance of surface preparation in ensuring the durability of concrete-grout interfaces.
DOI:
10.14359/51744378
23-096
May 1, 2024
Zoi G. Ralli and Stavroula J. Pantazopoulou
121
3
In light of the effort for decarbonization of the energy sector, it is believed that common geopolymer binding materials such as fly ash may eventually become scarce and new geological aluminosilicate materials should be explored as alternative binders in geopolymer concrete. A novel, tension-hardening geopolymer concrete (THGC) that incorporates high amounts of semi-reactive quarry wastes (metagabbro) as a precursor, and coarse quarry sand (granite) was developed in this study using geopolymer formulations. The material was optimized based on the particle packing theory and was characterized in terms of mechanical, physical, and durability properties (that is, compressive, tensile, and flexural resistance; Young’s modulus; Poisson’s ratio; absorption; drying shrinkage; abrasion; coefficient of thermal expansion; and chloride-ion penetration, sulfate, and salt-scaling resistance). The developed THGC, with an air-dry density of 1940 kg/m3 (121 lb/ft3), incorporates short steel fibers at a volume ratio of 2%, and is highly ductile in both uniaxial tension and compression (uniaxial tensile strain capacity of 0.6% at an 80% post-peak residual tensile strength). Using digital image correlation (DIC), multiple crack formation was observed in the strain-hardening phase of the tension response. In compression, the material maintained its integrity beyond the peak load, having attained 1.8% compressive strain at 80% postpeak residual strength, whereas upon further reduction to 50% residual strength, the sustained axial and lateral strains were 2.5% and 3.5%, respectively. The material exhibited low permeability to chloride ions and significant abrasion resistance due to the high contents of metagabbro powder and granite sand. The enhanced properties of the material, combined with the complete elimination of ordinary portland cement from the mixture, hold promise for the development of sustainable and resilient structural materials with low CO2 emissions, while also enabling the innovative disposal of wastes as active binding components.
10.14359/51740704
22-296
January 1, 2024
Xiaoqin Li, Li Zhang, Wenlu Wen, Shihua Li, and Xu Zhou
Engineered cementitious composites (ECCs) have excellent toughness and crack-control abilities compared to other cement-based materials, which can be used in underground and hydraulic engineering. Nevertheless, excellent impermeability and workability and low drying shrinkage are also required. Two groups of ECC mixture proportions with high fly ash-cement (FA/c) and watercement ratios (w/c) were chosen as baselines, and silica fume (SF) and a shrinkage-reducing agent (SRA) were introduced to improve the impermeability, workability, and mechanical behaviors. The workability laboratory evaluation indexes of ECC were also discussed. ECC mixture proportions with excellent workability (pumpability and sprayability), high toughness (ultimate tensile strain ɛtp over 3.5%), good impermeability (permeability coefficient K = 1.713 × 10–11 m/s), and low drying shrinkage (drying shrinkage strain ɛst = 603.6 × 10–6) were finally obtained. Then, flexural and shear tests were carried out for the material flexural/ shear strength and toughness evaluations, giving the characteristic material properties for the final ECC mixture proportions.
10.14359/51739200
22-388
December 1, 2023
R. M. Ghantous, V. Bui, S. Schaef, B. Fronczek, C. B. Jablonski, S. R. Reese, and W. J. Weiss
120
6
This study uses neutron radiography (NR) and visual inspection to quantify water penetration in concrete samples exposed to water pressure on one face. It provides experimental data regarding the impact of mixture proportions on the hydraulic permeability of concrete. Specifically, it illustrates the influence of water-cement ratio (w/c), curing duration, entrained air content, and coarse aggregate (CA) size and volume on water transport. In addition, this paper quantifies the impact of permeability-reducing admixtures (PRAs) on water transport in concrete. It was observed that decreasing the w/c and/or increasing the curing duration reduced the fluid transport. Liquid and powder PRAs efficiently reduced fluid transport in concrete without impacting the compressive strength. The liquid PRA showed more consistent results, likely due to better dispersion than the powder PRA. Fluid ingress in concrete samples appears to increase with entrained air content due to a lower degree of saturation (DOS) at the start of the test. Increasing the CA volume fraction or decreasing the CA size will increase the fluid transport in concrete due to an increase in the connectivity of the interfacial transition zone. The influence of entrained air content, curing duration, CA volume fraction, and CA size was less noticeable on mixtures with PRAs due to the higher density and low permeability of these samples compared to control samples.
10.14359/51739150
21-381
Othman AlShareedah and Somayeh Nassiri
Pervious concrete is a stormwater management practice used in the United States, Europe, China, Japan, and many other countries. Yet the design of pervious concrete mixtures to balance strength and permeability requires more research. Sphere packing models of pervious concrete were used in compressive strength testing simulations using the discrete element method with a cohesive contact law. First, three mixtures with varied water-cement ratios (w/c) and porosities were used for model development and validation. Next, an extensive database of simulated compressive strength and tested permeability was created, including 21 porosities at three w/c. Analysis of the database showed that for pavement applications where high permeability and strength are required, the advised porosity is 0.26 to 0.30, producing average strengths of 14.4, 11.1, and 7.7 MPa for w/c of 0.25, 0.30, and 0.35. The model can guide the mixture design to meet target performance metrics, save materials and maintenance costs, and extend the pavement life.
10.14359/51739157