Probabilistic Prediction Model for Flexure-Shear Capacity of Reinforced Concrete Girder (Prepublished)

International Concrete Abstracts Portal

  


Title: Probabilistic Prediction Model for Flexure-Shear Capacity of Reinforced Concrete Girder (Prepublished)

Author(s): Xinmin Zhang, Chaoyuan Wu, Zengwei Guo, Fanxiang Xia, Xianhu Ruan

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: Bayesian estimate; MCMC; probability model; RC member; shear capacity

DOI: 10.14359/51745491

Date: 12/19/2024

Abstract:
It is well known that the estimates of most shear capacity prediction models for reinforced concrete (RC) components are of high dispersion, due to its elaborate failure mechanism and elusive. A probability prediction model is more appropriate for estimating the shear capacity of RC members than a deterministic prediction model. Therefore, this study proposed a probabilistic model to evaluate the shear capacity of RC T-beams and employed a Bayesian-Markov Chain Monte Carlo (MCMC) approach to determine the posterior parameter in the shear strength prediction model by Bayesian updating. The analysis results indicate that the probabilistic model achieves minimal variance, offering the most accurate predictions that closely match test data compared with other prediction models. The shear capacity of the T-beam increases with changes in flange width and flange height ratio but remains constant once beyond a certain level. The shear capacity varies rapidly when the shear-span ratio (λ) is less than 2.5 or larger than 4.0, due to a notable shift in the failure mechanism. Besides, the shear capacity raises linearly by increasing the characteristic value of stirrups (ρvfyv).


Product unavailable, please call +1.248.848.3800



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer