Title: Prediction of Tensile Properties of Ultra-High-Performance Concrete Using Artificial Neural Network

Author(s): Amjad Y. Diab and Anca C. Ferche

Publication: Structural Journal

Volume: 121

Issue: 2

Appears on pages(s): 57-69

Keywords: artificial neural network (ANN); cracking stress; machine learning; multilayer perceptron (MLP); tensile strength; ultra-high-performance concrete (UHPC)

DOI: 10.14359/51740245

Date: 3/1/2024

Abstract:
A multilayer perceptron artificial neural network (MLP-ANN) was developed to calculate the cracking stress, tensile strength, and strain at tensile strength of ultra-high-performance concrete (UHPC), using the mixture design parameters and strain rate during testing as inputs. This tool is envisioned to provide reference values for direct tension test results performed on UHPC specimens, or to be employed as a framework to determine the tension response characteristics of UHPC in the absence of experimental testing, with minimal computational effort to determine the tensile characteristics. A database of 470 data points was compiled from 19 different experimental programs with the direct tensile strength, cracking stress, and strain at tensile strength corresponding to different UHPC mixtures. The model was trained, and its accuracy was tested using this database. A reasonably good performance was achieved with the coefficients of determination, R2, of 0.91, 0.81, and 0.92 for the tensile strength, cracking stress, and strain at tensile strength, respectively. The results showed an increase in the cracking tensile stress and tensile strength for higher strain rates, whereas the strain at tensile strength was unaffected by the strain rate.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer