Mechanical Characteristics of Hybrid-Fiber-Reinforced Concrete Shaft Wall Structure Under Uneven Load

International Concrete Abstracts Portal

  


Title: Mechanical Characteristics of Hybrid-Fiber-Reinforced Concrete Shaft Wall Structure Under Uneven Load

Author(s): Zhishu Yao, Yongjie Xu, Ping Zhang, Yu Fang, Chen Wang, Naihao Diao & Kun Hu

Publication: IJCSM

Volume: 17

Issue:

Appears on pages(s):

Keywords: uneven load, mine shaft wall, hybrid fibers, concrete, mechanical properties

DOI: 10.1186/s40069-022-00543-7

Date: 1/31/2023

Abstract:
To prevent damage to shaft walls in mines due to uneven loading, the mechanical properties of a shaft wall structure made of hybrid-fiber-reinforced concrete were studied. First, through orthogonal testing, the optimal mix proportion of the hybrid-fiber-reinforced concrete was obtained. Subsequently, a numerical calculation model of the shaft wall structure under uneven loading was established. The calculation results showed that the structure exhibits a tensile stress under the action of uneven loading and that its bearing capacity can be improved using the hybrid-fiber-reinforced concrete. Based on the numerical simulation results, a calculation formula for the bearing capacity of the shaft wall was obtained by regression. Finally, a model test was conducted on the shaft lining structure. The results obtained were consistent with those obtained using the numerical simulation regression formula, confirming the reliability of the numerical simulation results. This study showed that a hybrid-fiber-reinforced concrete shaft wall structure can better withstand uneven loads and has improved brittle failure characteristics. Hybrid-fiber-reinforced concrete is an excellent material for deep shaft wall structures.




  