Title: Generation of Optimal Load Paths for Corroded Reinforced Concrete Beams Part II: Multi-Angle Truss Model

Author(s): Lei Wang, Ping Yuan, and Royce W. Floyd

Publication: Structural Journal

Volume: 120

Issue: 4

Appears on pages(s): 115-126

Keywords: corroded reinforced concrete (CRC) beams; multi-angle truss model; multiple variable-inclination struts; optimal load paths; shear capacity

DOI: 10.14359/51738751

Date: 7/1/2023

Abstract:
A multi-angle truss model is proposed based on the optimal load paths of corroded reinforced concrete (CRC) beams. The load paths of CRC beams at the ultimate limit state, considering various corrosion levels, shear span-depth ratios, stirrup ratios, and loading methods are first studied. The load paths incorporating multiple variable-inclination struts can realistically describe the force-transfer mechanisms of CRC beams under flexure-shear interaction. The limiting failure criteria of the proposed truss model are then presented to estimate the shear capacity of CRC beams. Finally, the proposed model is verified by comparing with the experimental results of uncorroded and corroded reinforced concrete (RC) beams. Results show that the proposed model can reasonably predict the shear capacity and failure mode of CRC beams. For CRC beams at the ultimate limit state, corrosion damage has a negligible influence on the trajectory of load paths.The load paths change with the increase of the shear span-depth ratios of CRC beams.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer