Experimental Study on Column Reinforcing Bar Anchorage in Drilled Shaft Footings

International Concrete Abstracts Portal

  


Title: Experimental Study on Column Reinforcing Bar Anchorage in Drilled Shaft Footings

Author(s): Y. Yi, H. Kim, R. A. Boehm, Z. D. Webb, J. Choi, J. Murcia-Delso, T. D. Hrynyk, and O. Bayrak

Publication: Structural Journal

Volume: 120

Issue: 4

Appears on pages(s): 191-206

Keywords: bar anchorage; bond; critical section; development length; drilled shaft footing; large-scale tests; strut-and-tie method

DOI: 10.14359/51738721

Date: 7/1/2023

Abstract:
This paper presents an experimental study on the anchoragebehavior of column reinforcement subjected to tension in drilled shaft footings loaded under combined axial force and uniaxial bending moment. Large-scale tests were conducted on four footing specimens that were constructed with different column bar anchorage details: straight bars, hooked bars with two different hook orientations, and headed bars. All tension-loaded column reinforcement was shown to yield regardless of anchorage type. Further, all anchorage types developed stresses in the vicinity of the anchorage region except for bars with end hooks that were oriented outwards from the base of the column. Properly oriented hooked bars, considering the internal force flow of the strut-and-tie model, and headed bars developed more uniform stress distributions over their lengths as compared to straight bars. Based on developed stress distributions for the column reinforcement estimated fromstrain measurements, a critical section was also proposed to establish the anchorage requirement for the column reinforcement in a three-dimensional strut-and-tie model.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer