Title: Preparatory Study about Effect of Feldspar on Properties of Alkali-Activated Slag Concrete

Author(s): Alaa M. Rashad, Youssef A. Mosleh, and Mahmoud Gharieb

Publication: Materials Journal

Volume: 120

Issue: 2

Appears on pages(s): 53-63

Keywords: alkali-activated slag (AAS); compressive strength; feldspar; splitting strength; total porosity; water absorption

DOI: 10.14359/51737345

Date: 3/1/2023

Abstract:
In spite of feldspars being the most plentiful components in the crust of the earth, their uses in alkali-activated materials are still too limited. In this work, for the first time, the effect of different ratios of potassium feldspar on the properties of alkali-activated slag (AAS) concrete was studied. The slag was partially replaced with 10 to 50% feldspar with a stride of 10 wt. %. The effects of feldspar on the workability, compressive strength, splitting tensile strength, water absorption, and total porosity of AAS concrete were investigated. Different techniques were applied to investigate the crystalline phases, hydration products, and microstructures of the critical samples. The results showed a positive effect of feldspar on workability, of which the workability increased with increasing feldspar ratio. The incorporation of 10% feldspar has a positive effect on compressive strength, splitting tensile strength, water absorption, total porosity, and refining the microstructure, while higher ratios than 10% have a negative effect.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer