International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparison of Post-Tensioned Slabs with Banded-Uniform and Banded-Banded Tendon Arrangements

Author(s): Taye Ojo and Carin Roberts-Wollmann

Publication: Structural Journal

Volume: 119

Issue: 4

Appears on pages(s): 211-223

Keywords: banded-banded; flat plate; post-tensioned; prestressed; tendon; unbonded; uniform-banded

DOI: 10.14359/51734493

Date: 7/1/2022

Abstract:
This paper compares the flexural performance of two one-third-scale models of a two-way unbonded post-tensioned flat plate. One of the slabs had a conventional uniform-banded tendon arrangement and the other had a banded-banded tendon arrangement. The models had three bays in each direction and each bay was 10 x 10 ft (3 x 3 m). The specimens were tested using a whiffle tree system to approximate a uniformly distributed load, and were loaded to service and factored load multiple times, then loaded to failure. The performance of the banded-banded specimen was very similar to the uniform-banded specimen at service and factored load. The failure loads for the banded-banded and uniform-banded specimens were 310 and 321 lb/ft2 (14,840 and 15,380 N/m2) of total load, respectively—considerably higher than the design factored load of 197 lb/ft2 (9430 N/m2).


ALSO AVAILABLE IN: