Title: Seismic Performance of Hollow Bridge Pier Columns under Multi-Directional Loading

Author(s): Xuejian Liu, Rigoberto Burgueño, and Eric M. Hines

Publication: Structural Journal

Volume: 118

Issue: 5

Appears on pages(s): 101-113

Keywords: column; ductility; high-strength concrete (HSC); load path; multi-directional; pier; shear capacity; web crushing

DOI: 10.14359/51732829

Date: 9/1/2021

Abstract:
High-strength concrete (HSC) offers the potential of enhancing flexure-shear displacement ductility capacity of reinforced concrete hollow bridge pier columns with highly reinforced boundary elements and slender wall webs exhibiting three-dimensional (3-D) inelastic web crushing shear failure mechanisms. In this study, the seismic performance of HSC bridge pier columns was evaluated through tests on two large-scale hollow pier column units subjected to a diagonal and a multi-directional cyclic loading protocol with design concrete compressive strengths of 34 and 138 MPa (5 and 20 ksi), respectively. Both test units exhibited ductile flexure-shear behavior until web crushing occurred at moderate ductility levels. The 3-D inelastic web crushing shear performance was evaluated based on test observations and the hysteretic force-displacement behavior along principal and diagonal directions. To evaluate the loading path effect on the inelastic web crushing shear performance specifically, the degradation of shear stiffness and energy dissipating capacity were quantified and compared with a two-dimensional (2-D) plane pier wall test. The comparable displacement ductility capacity of the two test units shows that HSC improves web crushing performance of the pier columns through smeared web concrete damage and shear stiffness degradation under multi-directional loading.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer