Title: Biaxial Principal Stress Interaction Diagram for Reinforced Concrete Membrane Elements

Author(s): Ahmad Rahimian

Publication: Structural Journal

Volume: 116

Issue: 3

Appears on pages(s): 119-133

Keywords: biaxial stress; interaction diagram; limit state; membrane elements; principal stress; reinforced concrete; shear stress; shell elements

DOI: 10.14359/51714474

Date: 5/1/2019

Abstract:
Advancements in finite element methods and research related to reinforced concrete (RC) elements have greatly facilitated the analysis and design of today’s increasingly complex concrete structures. However, the design criteria for shell elements under membrane actions are not explicitly identified in ACI 318-14. This paper presents an approach based on an interaction diagram of principal stresses to supplement the design of RC shell elements under membrane stresses. It provides a closed-form solution for creating the ultimate limit state boundary for an RC membrane element under biaxial and shear stresses. These boundary limits can then be used to evaluate the adequacy of the RC element for the applied loads. The proposed method is based on the well-known shear theories of the rotating angle softened truss model while considering aspects of the Modified Compression Field Theory and the concrete limit state under biaxial compression.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer