Evaluation of Mechanical and Durability Properties of Sulfur Concrete

International Concrete Abstracts Portal

  


Title: Evaluation of Mechanical and Durability Properties of Sulfur Concrete

Author(s): Renata Kotynia, Radoslaw Walendziak, and Michal Lewandowski

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 118.1-118.10

Keywords: combustion products, durability, freeze-thaw resistance, sulfur concrete, sulfur polymer, strength

DOI: 10.14359/51711101

Date: 8/10/2018

Abstract:
The paper presents research on sulfur concrete designed with the following combustion products: fly ash, slag and phospho-gypsum. The purpose of this investigation was to evaluate characteristics of sulfur concrete, including its mechanical and durability properties. It was established that mechanical characteristics of sulfur concrete will correspond with those of cement concrete used in the production of small precast members used in civil engineering, hydraulic engineering, road constructions, structures exposed to aggressive environments especially chemical industry, petroleum industry, food industry and farming. The test results confirmed low water absorption, high resistance to wear abrasion, high freeze-thaw scaling resistance (surface weathering) in a salty environment and high compressive and tensile strength of individual compositions. However, the tests results did not confirm the freeze-thaw resistance of the sulfur concrete specimens due to low freeze-thaw resistance of sulfur binders. Further research is needed to increase the freeze-thaw attack resistance of the sulfur polymer to provide the proper resistance of the final sulfur concrete products.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer