Title: Using Self-Consolidating Concrete for Bridge Repairs

Author(s): H. Celik Ozyildirim and Gail M. Moruza

Publication: Concrete International

Volume: 37

Issue: 4

Appears on pages(s): 42-46

Keywords: admixtures, formwork, placement, shotcrete

DOI:

Date: 4/1/2015

Abstract:
Bridge substructure repairs that were completed using self-consolidating concrete (SCC) are described. The Virginia Department of Transportation (VDOT) has successfully used SCC on bridge repair projects for about 5 years. Placement and testing requirements for SCC are similar to those for conventional concrete, the required formwork provides initial protection against moisture loss, and the finish can be as smooth as the formwork surface. Completed repairs show that SCC can be successfully placed, and the finished product has minimal cracking.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer