Title: Concrete Q & A: Popouts or Popoffs?
Author(s):
Publication: Concrete International
Volume: 35
Issue: 12
Appears on pages(s): 88
Keywords:
DOI:
Date: 12/1/2013
Abstract: My concrete driveway was placed last year in the fall. This summer, I noticed that small concrete fragments have broken off the driveway surface exposing large pieces of aggregate. Can you tell me what might have caused this issue? Should I worry about further deterioration?