Title: Two-Parameter Kinematic Theory for Shear Behavior of Deep Beams

Author(s): Boyan I. Mihaylov, Evan C. Bentz, and Michael P. Collins

Publication: Structural Journal

Volume: 110

Issue: 3

Appears on pages(s): 447-456

Keywords: deep beams; kinematics; shear; size effect; ultimate deformations

DOI: 10.14359/51685602

Date: 5/1/2013

Abstract:
This paper presents a kinematic model for deep beams capable of describing the deformed shape of such members in terms of just two primary parameters. The kinematic model is combined with equilibrium equations and stress-strain relationships to form a theory to predict the shear strength and deformations patterns of deep beams at shear failure. These deformation patterns include crack widths, maximum deflections, and the complete displacement field for the beam. The kinematic theory predicts the components of shear strength of deep beams and how they vary with a/d ratio. These components indicate a significant size effect for the shear strength of deep beams, even for members with transverse reinforcement. The theory has been validated against a large number of experimental results.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer