Abstract:
A numerical technique based on the theory of plasticity is developed to predict an optimum failure surface generatrix and concrete breakout capacity of single anchors away from edges under tensile loads. Concrete is regarded as a rigid, perfectly plastic material obeying a modified coulomb failure criteria with effective compressive and tensile strengths. The failure mode is idealized as an assemblage of two rigid blocks separated by failure surfaces of displacement discontinuity. Minimization of the collapse load predicted by the energy equation produces the optimum shape of the failure surface generatrix. A simplified solution is also developed by approximating the failure surface as two straight lines. The effect of different parameters on the concrete breakout capacity of anchors is reviewed using the developed mechanism analysis, ACI 318-05, and test results of 501 cast-in-place and 442 post-installed anchor specimens. The shape of failure surface and concrete breakout capacity of anchors predicted by the mechanism analysis are significantly affected by the ratio between effective tensile and compressive strengths of concrete. For anchors installed in concrete having a low ratio between effective tensile and compressive strengths, a much larger horizontal extent of failure planes in concrete surface is predicted by the mechanism analysis than recommended by ACI 318-05, similar to test results. Experimental concrete breakout capacity of anchors is closer to the prediction obtained from the mechanism analysis than ACI 318-05. ACI 318-05 provisions for anchors sharply underestimate the breakout capacity of cast-in-place and post-installed anchors having effective embedment depths exceeding 200 and 80 mm (7.87 to 3.15 in.), respectively, installed in concrete of compressive strength larger than 50 MPa (7250 psi).


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer