Title: Shear and Moment Transfer between Concrete Slabs and Columns

Author(s): Hanson, N. W., and Hanson, J. M.

Publication: Commentary Reference

Volume: 11

Issue: 68

Appears on pages(s): pp. 2-16

Keywords:

DOI:

Date: 6/1/2005

Abstract:
Journal, PCA Research and Development Laboratories, V. 10, No. 1, Jan. 1968




  