Title: Influence of Aggregate Size on Strain-Rate Tensile Behavior of Concrete

Author(s): Ezio Cadoni, Kamel Labibes, Mario Berra, Marco Giangrasso, and Carlo Albertini

Publication: Materials Journal

Volume: 98

Issue: 3

Appears on pages(s): 220-223

Keywords: aggregate; cement, portland; dynamic loading; strain; stress; tensile.

DOI: 10.14359/10276

Date: 5/1/2001

Abstract:
The study of the concrete behavior over a large range of strain rates was the aim of a broad research project conducted at the Joint Research Center-Ispra (Italy). The program was developed to produce new data concerning a few basic but debated subjects of industrial importance. This paper describes the influence of the increasing aggregate size on the strain-rate tensile behavior of plain concrete.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer