On the and shirkage testing of concrete
Author(s):
Agullo, L.; Aguado de Cea, A.; Aparicio Bengoechea, A.C.
Publication:
ACHE
Volume:
45
Issue:
190
Appears on pages(s):
59 - 66
Keywords:
DOI:
Date:
1/1/1994
Abstract:
Tjis paper first describes the creep and shrinkage tests of concrete for the Alamillo bridge (Sevilla, EXPO-92). Next, the test results are analysed for the fluence of instantaneous strain on creep strain. Finally, the test results are compared with analytical results obtained following the Spanish code EP-93.