Title:
Mixing Water Control by Use of a Moisture Meter
Author(s):
C. B. Van Alstine
Publication:
Journal Proceedings
Volume:
52
Issue:
11
Appears on pages(s):
341-347
Keywords:
no keywords
DOI:
10.14359/11604
Date:
11/1/1955
Abstract:
Conditions at Reservoir No. 22 Dam created severe fluctuations of free moisture in sand and pea gravel. Use of a moisture meter as a basis for ad-justments in water is described. Charts show the effectiveness of the device, in conjunction with other control measures, as an aid to producing quality concrete.