Title: Can Artificial Intelligence Improve Nondestructive Evaluation of Concrete Strength?

Author(s): Seyed Alireza Alavi, Martin Noël, Hamed Layssi, and Farid Moradi

Publication: Concrete International

Volume: 46

Issue: 5

Appears on pages(s): 51-56

Keywords: model, prediction, method, evaluation

DOI:

Date: 5/1/2024

Abstract:
Adoption of artificial intelligence (AI) for civil engineering applications has been relatively slow but is beginning to garner increasing attention through demonstration of practical use cases. This article explores the extent to which AI can be integrated with the SonReb method for nondestructive evaluation of concrete compressive strength in reinforced concrete structures.




  