Showing 1-5 of 6 Abstracts search results
|
Wael A. Zatar, M. Ammar Alzarrad, Tu T. Nguyen, and Hai D. Nguyen
In this paper, the artificial neural network (ANN) method is utilized to predict ground-penetrating radar reflection amplitudes from four different inputs, namely, temperature, ambient relative humidity, chloride level, and corrosion condition on the surface of the reinforcing bar. A total of 288 ground penetrating radar (GPR) data points were collected from a series of chloride-contaminated concrete slabs under various environmental profiles that were used to train, validate, and test the proposed ANN model. The ANN model performed well in predicting the GPR reflection signals, with the overall coefficient of determination (R2) being 0.9958. The overall mean squared error (MSE) and root mean squared error (RSME) values are 0.015 and 0.122, respectively. These values are very low, which means that the ANN model has an excellent prediction capability. The research results show that the GPR reflection amplitudes are more sensitive to the temperature changes and chloride level parameters than the ambient relative humidity and rust condition on the reinforcing bar surface. Using the ANN method to predict the GPR reflection amplitudes is relatively new for structural concrete applications. This study paves the way for further developments of neural networks in civil and structural engineering.
|
|
The first international FRC workshop supported by RILEM and ACI was held in Bergamo (Italy) in 2004. At that time, a lack of specific building codes and standards was identified as the main inhibitor to the application of this technology in engineering practice. The workshop aim was placed on the identification of applications, guidelines, and research needs in order for this advanced technology to be transferred to professional practice.
The second international FRC workshop, held in Montreal (Canada) in 2014, was the first ACI-fib joint technical event. Many of the objectives identified in 2004 had been achieved by various groups of researchers who shared a common interest in extending the application of FRC materials into the realm of structural engineering and design. The aim of the workshop was to provide the State-of-the-Art on the recent progress that had been made in term of specifications and actual applications for buildings, underground structures, and bridge projects worldwide. The rapid development of codes, the introduction of new materials and the growing interest of the construction industry suggested presenting this forum at closer intervals. In this context, the third international FRC workshop was held in Desenzano (Italy), four years after Montreal. In this first ACI-fib-RILEM joint technical event, the maturity gained through the recent technological developments and large-scale applications were used to show the acceptability of the concrete design using various fibre compositions. The growing interests of civil infrastructure owners in ultra-high-performance fibre-reinforced concrete (UHPFRC) and synthetic fibres in structural applications bring new challenges in terms of concrete technology and design recommendations. In such a short period of time, we have witnessed the proliferation of the use of fibres as structural reinforcement in various applications such as industrial floors, elevated slabs, precast tunnel lining sections, foundations, as well as bridge decks. We are now moving towards addressing many durability-based design requirements by the use of fibres, as well as the general serviceability-based design. However, the possibility of having a residual tensile strength after cracking of the concrete matrix requires a new conceptual approach for a proper design of FRC structural elements. With such a perspective in mind, the aim of FRC2018 workshop was to provide the State-of-the-Art on the recent progress in terms of specifications development, actual applications, and to expose users and researchers to the challenges in the design and construction of a wide variety of structural applications. Considering that at the time of the first workshop, in 2004, no structural codes were available on FRC, we have to recognize the enormous work done by researchers all over the world, who have presented at many FRC events, and convinced code bodies to include FRC among the reliable alternatives for structural applications. This will allow engineers to increasingly utilize FRC with confidence for designing safe and durable structures. Many presentations also clearly showed that FRC is a promising material for efficient rehabilitation of existing infrastructure in a broad spectrum of repair applications. These cases range from sustained gravity loads to harsh environmental conditions and seismic applications, which are some of the broadest ranges of applications in Civil Engineering. The workshop was attended by researchers, designers, owner and government representatives as well as participants from the construction and fibre industries. The presence of people with different expertise provided a unique opportunity to share knowledge and promote collaborative efforts. These interactions are essential for the common goal of making better and sustainable constructions in the near future.
The workshop was attended by about 150 participants coming from 30 countries. Researchers from all the continents participated in the workshop, including 24 Ph.D. students, who brought their enthusiasm in FRC structural applications.
For this reason, the workshop Co-chairs sincerely thank all the enterprises that sponsored this event. They also extend their appreciation for the support provided by the industry over the last 30 years which allowed research centers to study FRC materials and their properties, and develop applications to making its use more routine and accepted throughout the world. Their important contribution has been essential for moving the knowledge base forward.
Finally, we appreciate the enormous support received from all three sponsoring organizations of ACI, fib and Rilem and look forward to paving the path for future collaborations in various areas of common interest so that the developmental work and implementation of new specifications and design procedures can be expedited internationally.
June 2018
Bruno Massicotte, Fausto Minelli, Barzin Mobasher, Giovanni Plizzari
|
|
Editors: Mario Alberto Chiorino, Luigi Coppola, Claudio Mazzotti, Roberto Realfonzo, Paolo Riva
With the dawn of twenty-first century, the world has entered into an era of sustainable development. The main challenge for concrete industry is to serve the two major needs of human society, the protection of the environment, on one hand, and - on the other hand - meeting the infrastructural requirements of the world growing population as a consequence of increase in both industrialization and urbanization. In the past, concrete industry has satisfied these needs well. Concrete is an environmentally friendly material useful for the construction of vast infrastructures. Skyscrapers, highway bridges, roads, water retaining structures and residential buildings are all testimonials to concrete’s use and versatility. However, for a variety of reasons the situation has changed dramatically in the last years. First of all, the concrete industry is the largest consumer of natural resources. Secondly, portland cement, the binder of modern concrete mixtures, is not as environmentally friendly. The world’s portland cement production, in fact, contributes to the earth’s atmosphere about 7% of the total CO2 emissions, CO2 being one of the primary greenhouse gases responsible for global warming and climate change. As a consequence, concrete industry in the future has to face two antithetically needs. In other words how the concrete industry can feed the growing population needs being – at the same time - sustainable?
ACI Italy Chapter has been playing a significant role in the last years in the broad area of concrete technology in Italy and, in particular, in the field of concrete durability and sustainability. ACI Italy Chapter has become increasingly involved in research and development dealing with durability and sustainability issues such as reduction in CO2 emissions, use of recycled materials and innovative products, design of durable structures and maintenance, repair and refurbishment of concrete infrastructures.
In October 2015, the American Concrete Institute Italy Chapter (ACI IC) and the Department of Civil, Chemical, Environmental, and Material Engineering (DICAM) of the University of Bologna sponsored the First International Workshop on “Durability & Sustainability of Concrete Structures” in Bologna (Italy). The workshop was co-sponsored by the American Concrete Institute and ACI Committee 201. The proceedings of the workshop were published by ACI IC as SP305. The proceedings consist of forty-eight refereed papers concerning reduction in green house gases in cement and concrete industry, recycled materials, innovative binders and geopolymers, Life Cycle Cost Assessment in concrete construction, reuse and functional resilience of reinforced concrete structures, repair and maintenance, testing, inspection and monitoring.
Many thanks are extended to the members of the technical paper review panel. Without their dedicated efforts it would not have been possible to publish the proceedings. The cooperation of the authors in accepting reviewers’ comments and suggestions and in revising the manuscripts accordingly is greatly appreciated.
Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order.
SP-305
|
|
The Industrial Revolution in the middle of the 18th century determined mankind’s destiny. The mass production of goods increased the population at an accelerated rate, and, consequently, mankind is facing the risk of natural resources and energy depletion. The greatest challenge to mankind in this century is to ensure the sustainability of the “inhabitants” of the Earth. The basis of mankind’s social and economic activities is infrastructure and buildings. As a result, the construction industry has a far greater influence on the sustainability of mankind and the Earth. Unfortunately, the construction industry has little appreciation of these facts. In order to change from the “old” industry to a “new” industry, the concept of “sustainability” should be introduced as a fundamental idea. The fundamental aspects for considering the sustainability of mankind and the Earth are society, economy, and environment. The essence of the construction industry can be appreciated from these views. There exists interconnection among safety, cost, and environmental impact. In the existing “old” construction engineering, this interconnection is not dealt with systematically. This paper outlines the background on the necessity to introduce a “sustainability” philosophy into the construction sector and proposes a basic framework for sustainability design as a “new” design system
|
|
H.C. Mertol, S. Rizkalla, P. Scott, J.M. Lees,
and R. El-Hacha
The need for sustainable structures is the driving force for the growing international interest in using advanced materials such as fiber reinforced polymer (FRP) materials for civil infrastructure applications. To date, FRP materials have not realized their full potential within the construction industry. One of the contributing factors is the limited information regarding their long-term performance. In particular, since the service life of a civil engineering structure is typically 50 to 100 years, knowledge of the long-term durability of FRPs is of prime importance. The research work presented in this paper is the result of a research collaboration between North Carolina State University and the University of Cambridge. The research investigates the durability of concrete beams prestressed with CFRP bars and compares the results with those of companion beams prestressed with steel wires. A total of 15 beams have been constructed and tested under different mechanical and environmental conditions. The parameters included in the program were the level of sustained stress in the bars and wires (55 and 70 percent of the ultimate bar or wire strength), the environmental exposure condition (air exposure and continuous exposure to 15 percent by mass salt water spray at 54 °C temperature), the length of time under sustained load (9 and 18 months) and the method of testing (with or without application of cyclical loading prior to static testing to failure). The experimental program illustrates that CFRP prestressed concrete beams exhibit comparable ultimate strength and fatigue strength properties in comparison to equivalent steel prestressed concrete beams. Furthermore, test results show that the beams prestressed with steel wires did not survive the environmental exposure over 12 months whereas the beams prestressed with CFRP bars survived up to the end of the 18 month long extreme environmental exposure, indicating the excellent durability of CFRP in the marine environment. Provided that provision is made for the lack of CFRP ductility in comparison to steel, the research undertaken has indicated that CFRP prestressed concrete is a durable, appropriate option when designing structures for use in offshore environments.
|
|