Title:
Second Progress Report-Continuously Reinforced Concrete Pavements
Author(s):
J. D. Lindsay
Publication:
Journal Proceedings
Volume:
59
Issue:
11
Appears on pages(s):
1569-1586
Keywords:
none
DOI:
10.14359/7965
Date:
10/1/1962
Abstract:
This progress report presents brief data on the design and performance of recently constructed continuously reinforced concrete pavements constructed in Michigan, Maryland, Texas, Wisconsin, Maine, and Pennsylvania. Included are a description of experimental special terminal joint provisions and end anchorages, a summary of theoretical developments for selection of slab thickness and reinforcement, and a summary of present recommendations for design. The report concludes with recommendations for future research.