ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Discussion from the July-August 2014 ACI Structural Journal

Author(s): Rafael Alves de Souza and Sergio Breña; Jian Yuan; and Rafael Alves de Souza and Sergio Breña

Publication: Structural Journal

Volume: 112

Issue: 3

Appears on pages(s): 407-412

Keywords:

DOI: 10.14359/51687861

Date: 5/1/2015

Abstract:
Disc. 111-S60/From the July-August 2014 ACI Structural Journal, p. 731 Depth Effect in Deep Beams. Paper by David B. Birrcher, Robin G. Tuchscherer, Matt Huizinga, and Oguzhan Bayrak; Disc.111-S67/From the July-August 2014 ACI Structural Journal, p. 809 Shear Strength of Reinforced Concrete Beams. Paper by Wu Wei Kuo, Thomas T. C. Hsu, and Shyh Jiann Hwang; and Disc. 111-S73/From July-August 2014 ACI Structural Journal, pp.873-880 Experimental Evaluation of Strut-and-Tie Model of Indeterminate Deep Beam. Paper by D. B. Garber, J. M. Gallardo, G. D. Huaco, V. A. Samaras, and J. E. Breen