Title: Concrete with Very High Resistance to Chloride Ingress

Author(s): Susanto Teng, Bahador Sabet Divsholi, Tze Yang Darren Lim, and Odd E. Gjørv

Publication: Concrete International

Volume: 36

Issue: 5

Appears on pages(s): 30-36

Keywords: corrosion, diffusivity, permeability, strength

Date: 5/1/2014

Abstract:
Researchers at Nanyang Technological University in Singapore are examining a possibility of constructing offshore concrete structures extending from the seabed to above sea level. The upper portion of these structures would serve as new land while the volumes captured below the sea level could be used for storage tanks or other industrial purposes. These structures will require concrete mixtures with very high resistance to chloride ingress. Potential mixtures are discussed.

Registered Subscribers »   View the full article.

Not an online Journal subscriber? Click here to subscribe.

This product is available for purchase and download.  Click on the Add To Cart button to continue.