Product Detail

Chloride Transport Measurements for a Plain and Internally Cured Concrete Mixture

Price: $ 19.50 USD

Choose Product Language

Choose Product Units


Choose Product Format


 

Document Details

Document Name: SP290-14

Periodical: Special Publication

Authors: Carmelo Di Bella, Chiara Villani, Elizabeth Hausheer and Jason Weiss

Date: September 14, 2012

Volume: 290

Pages: 1-16

Type: Special Publication

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).