Title: In-Transit Water Additions to Concrete

Author(s): Eric P. Koehler

Publication: Concrete International

Volume: 35

Issue: 8

Appears on pages(s): 65-67

Keywords: automated, slump, water content, mixing truck

Date: 8/1/2013

Abstract:
ASTM C94/C94M, “Standard Specification for Ready-Mixed Concrete,” has recently been revised to allow water additions to mixing trucks as they travel from the batching plant to the job site. These changes were facilitated by new technology that allows automated evaluation of slump and automated control of water additions. Concrete producers, engineers, and contractors can expect reduced variability and increased productivity.

Not an online Journal subscriber? Click here to subscribe.

This product is available for purchase and download.  Click on the Add To Cart button to continue.