Title: A Design Alternative for Floor Art

Author(s): Steven H. Miller

Publication: Concrete International

Volume: 35

Issue: 3

Appears on pages(s): 60-62

Keywords: polished, color, adhesive, testing, aggregate

Date: 3/1/2013

Abstract:
To decorate polished concrete floors, liquid dyes are applied by a sprayer to create a random pattern and even distribution of color. Laser-cut, thin, adhesive stencils are used to produce highly intricate, artistic works; and multilayer stencils can be used to create three-dimensional illusions. These techniques, including surface preparation and testing, are described.

Not an online Journal subscriber? Click here to subscribe.

This product is available for purchase and download.  Click on the Add To Cart button to continue.