Repeatability and Pervasiveness of Self-Healing in Engineered Cementitious Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Repeatability and Pervasiveness of Self-Healing in Engineered Cementitious Composites

Author(s): Mustafa Sahmaran, Gürkan Yildirim, Rezhin Noori, Erdogan Ozbay, and Mohamed Lachemi

Publication: Materials Journal

Volume: 112

Issue: 4

Appears on pages(s): 513-522

Keywords: engineered cementitious composite (ECC); repeatability; selfhealing; supplementary cementitious material (SCM)

DOI: 10.14359/51687308

Date: 7/1/2015

Abstract:
This paper investigates the intrinsic self-healing ability of engineered cementitious composites (ECCs) coupled with multiple microcrack formation under mechanical loading based on two robustness criteria: repeatability and pervasiveness. To this end, two different composites containing Class F fly ash and slag were investigated. To generate microcracks, specimens were repeatedly preloaded up to 70% of their deformation capacities under mechanical loading at the end of each specified cyclic wet/dry conditioning period. Resonant frequency (RF) and rapid chloride permeability tests (RCPT) were used to assess the extent of damage and self-healing, and final results were supported by microscope observations. RF measurements were recorded from two different parts of each specimen (the top and middle portions) to monitor whether self-healing takes place in certain regions or whether it is pervasive over the entire specimen. Results of the experimental study show that depending on the type of mineral admixture used and the duration of initial curing before deterioration, ECC specimens can recover up to 85% of their initial RF measurements, even after six repetitive preloading applications. The recovery rates observed in the middle portion are similar to those in the top portion for both ECC mixtures (to a slightly lesser extent), which implies that self-healing is quite pervasive. Furthermore, after repeated application of severe preloading, RCPT results for both mixtures satisfy low or moderate chloride ion penetrability levels in accordance with ASTM C1202. Due to the enhanced self-healing capability of specimens, maximum crack width observed over the specimen surfaces was restricted to 190 µm (0.008 in.), even after nine preloadings. These findings suggest that under certain conditions, the ECC materials produced in this study may significantly enhance the functionality of structures by reducing the need for repair and/or maintenance.

Related References:

1. Mather, B., and Warner, J., “Why Do Concrete Repairs Fail?” interview held at University of Wisconsin, Department of Engineering Professional Development, Madison, WI, Nov. 5, 2004.

2. Mihashi, H.; Kaneko, Y.; Nishiwaki, T.; and Otsuka, K., “Fundamental Study on Development of Intelligent Concrete Characterized by Self-Healing Capability for Strength,” Japan Concrete Institute, V. 22, No. 2, 2000, pp. 441-450.

3. Huang, H., and Ye, G., “Application of Sodium Silicate Solution as Self-Healing Agent in Cementitious Materials,” International Conference on Advances in Construction Materials through Science and Engineering, 2011, Hong Kong, pp. 530-536.

4. Jonkers, H. M., “Bacteria-Based Self-Healing Concrete,” HERON, V. 56, No. 1/2, 2011, pp. 1-12.

5. Kishi, T.; Ahn, T. H.; Hosoda, A.; and Takaoka, H., “Self-Healing Behavior by Cementitious Recrystallization of Cracked Concrete Incorporating Expansive Agent,” First International Conference on Self-Healing Materials, Delft, the Netherlands, Apr. 18-20, 2007.

6. Ahn, T. H., and Kishi, T., “Crack Self-Healing Behavior of Cementitious Composites Incorporating Various Mineral Admixtures,” Advanced Concrete Technology, V. 8, No. 2, 2010, pp. 171-186. doi: 10.3151/jact.8.171

7. Şahmaran, M., and Li, V. C., “Engineered Cementitious Composites: Can They Be Accepted as a Crack-Free Concrete?” Transportation Research Record, V. 2164, 2010, pp. 1-8. doi: 10.3141/2164-01

8. Li, V. C., and Herbert, E., “Robust Self Healing Concrete for Sustainable Infrastructure,” Advanced Concrete Technology, V. 10, No. 6, 2012, pp. 207-218. doi: 10.3151/jact.10.207

9. Li, V. C., and Yang, E., “Self Healing in Concrete Materials,” Self Healing Materials, Springer Netherlands, Dordrecht, the Netherlands, 2007, pp. 161-190.

10. Yang, Y.; Lepech, M. D.; Yang, E. H.; and Li, V. C., “Autogenous Healing of Engineered Cementitious Composites under Wet-Dry Cycles,” Cement and Concrete Research, V. 39, No. 5, 2009, pp. 382-390. doi: 10.1016/j.cemconres.2009.01.013

11. Li, V. C., “Engineered Cementitious Composites Tailored Composites through Micromechanical Modeling,” Fiber Reinforced Concrete: Present and the Future, N. Banthia, A. Bentur, and A. Mufti, eds., Canadian Society for Civil Engineering, Montreal, QC, Canada, 1997, pp. 64-97.

12. Maalej, M.; Hashida, T.; and Li, V. C., “Effect of Fiber Volume Fraction on the Off-Crack Plane Fracture Energy in Strain-Hardening Engineered Cementitious Composites,” Journal of the American Ceramic Society, V. 78, No. 12, 1995, pp. 3369-3375. doi: 10.1111/j.1151-2916.1995.tb07979.x

13. ASTM C215-08, “Standard Test Method for Fundamental Transverse, Longitudinal, and Torsional Frequencies of Concrete Specimens,” ASTM International, West Conshohocken, PA, 2008, 7 pp.

14. ASTM C1202-12, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2012, 7 pp.

15. Jacobsen, S., and Sellevold, E. J., “Self Healing of High Strength Concrete after Deterioration by Freeze/Thaw,” Cement and Concrete Research, V. 26, No. 1, 1996, pp. 55-62. doi: 10.1016/0008-8846(95)00179-4

16. Jiang, Z.; Sun, Z.; and Wang, P., “Internal Relative Humidity Distribution in High-Performance Cement Paste Due to Moisture Diffusion and Self Desiccation,” Cement and Concrete Research, V. 36, No. 2, 2006, pp. 320-325. doi: 10.1016/j.cemconres.2005.07.006

17. Sahmaran, M.; Yucel, H. E.; Demirhan, S.; Arik, M. T.; and Li, V. C., “Combined Effect of Aggregate and Mineral Admixtures on Tensile Ductility of Engineered Cementitious Composites,” ACI Materials Journal, V. 109, No. 6, Nov.-Dec. 2012, pp. 627-638.

18. Song, G., and van Zijl, G. P. A. G., “Tailoring ECC for Commercial Application,” 6th International RILEM Symposium on Fiber Reinforced Concrete, RILEM Publications SARL, Bagneux, France, 2004, pp. 1391-1400.

19. Shehata, M. H.; Thomas, M. D. A.; and Bleszynski, R. F., “The Effect of Fly Ash Composition on the Chemistry of Pore Solution in Hydrated Cement Pastes,” Cement and Concrete Research, V. 29, No. 12, 1999, pp. 1915-1920. doi: 10.1016/S0008-8846(99)00190-8

20. Sahmaran, M.; Yildirim, G.; and Erdem, T. K., “Self-Healing Capability of Cementitious Composites Incorporating Different Supplementary Cementitious Materials,” Cement and Concrete Composites, V. 35, No. 1, 2013, pp. 89-101. doi: 10.1016/j.cemconcomp.2012.08.013

21. Gagné, R., and Argouges, M., “A Study of the Natural Self-Healing of Mortars using Air-Flow Measurements,” Materials and Structures, V. 45, No. 11, 2012, pp. 1625-1638. doi: 10.1617/s11527-012-9861-y

22. Aldea, C.; Song, W.; Popovics, J. S.; and Shah, S. P., “Extent of Healing of Cracked Normal Strength Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 12, No. 1, 2000, pp. 92-96. doi: 10.1061/(ASCE)0899-1561(2000)12:1(92)

23. Clear, C. A., The Effects of Autogenous Healing upon the Leakage of Water through Cracks in Concrete, Cement and Concrete Association, Wexham Springs, UK, 31 pp.

24. Edvardsen, C., “Water Permeability and Autogenous Healing of Cracks in Concrete,” ACI Materials Journal, V. 96, No. 6, Nov.-Dec. 1999, pp. 448-455.


ALSO AVAILABLE IN: