Experimental Study for Class B Lap Splice of 600 MPa (87 ksi) Reinforcing Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study for Class B Lap Splice of 600 MPa (87 ksi) Reinforcing Bars

Author(s): Won-Seok Choi, Hong-Gun Park, Lan Chung, and Jin-Keun Kim

Publication: Structural Journal

Volume: 111

Issue: 1

Appears on pages(s): 49-58

Keywords: bond; Class B splice; high-strength steel; splice length

DOI: 10.14359/51686429

Date: 1/1/2014

Abstract:
An experimental study was performed to evaluate the applicability of ACI 318 to the Class B splice of 600 MPa (87 ksi) reinforcing bars. Twelve simply supported beams and slabs with reinforcing bar splices were tested under monotonic loading. The test parameters were the reinforcing bar diameter, concrete cover thickness, concrete strength, and stirrup spacing. Concrete strengths ranged from 24.7 to 55.3 MPa (3582 to 8021 psi). Most of the specimens were designed to satisfy the Class B splice length specified by ACI 318. The average bar stresses resulting from this test were compared with the predictions by the ACI 318 provisions. The results showed that the reinforcing bar splices gave a satisfactory performance for all D13 (diameter = 13 mm [0.51 in.]) bar splices. For D22 and D32 bars, the use of either transverse reinforcement or thick concrete cover was recommended to develop the specified yield strength of 600 MPa (87 ksi). The test results were also compared with the predictions by the ACI 408R 03 and Eurocode 2 provisions.


ALSO AVAILABLE IN:

Electronic Structural Journal