Abstract:
Appropriate curing is important in the development of required compressive strength and durability properties in concrete. Conventional concrete practices require a selection of effective and cost-efficient curing techniques to achieve well-hydrated, uniform, and dense microstructure within available resources. An experimental program was designed to study the hydration of concrete under various conventional and unconventional curing techniques. Different curing techniques were investigated comprising water, burlap, liquid membrane-forming compound, combinations of admixtures, and liquid membrane-forming compound, admixtures, and burlap compared to ambient curing. Additionally, internal curing methods comprising prewetted lightweight aggregate (LWA), super-absorbent polymers (SAPs), and shrinkagereducing admixtures were investigated. Microstructural development related to compressive strength at different ages were considered to monitor the effect of various curing methods on microstructure and strength development in concrete. The findings are helpful in establishing the best curing techniques to obtain optimum strength and durability properties in concrete using available resources.
Related References:
1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.
2. ACI Committee 305, “Guide to Hot Weather Concreting (ACI 305R-10),” American Concrete Institute, Farmington Hills, MI, 2010, 23 pp.
3. Al-Gahtani, A. S., “Effect of Curing Methods on the Properties of Plain and Blended Cement Concretes,” Construction and Building Materials, V. 24, No. 3, 2010, pp. 308-314. doi: 10.1016/j.conbuildmat.2009.08.036
4. Yilmaz, U. S., and Turken, H., “The Effects of Various Curing Materials on the Compressive Strength Characteristic of the Concretes Produced with Multiple Chemical Admixtures,” Scientia Iranica, V. 19, No. 1, 2012, pp. 77-83. doi: 10.1016/j.scient.2011.11.038
5. Krishna, R.; Kumar, R. P.; and Khan, A. M., “A Study on the Influence of Curing on the Strength of a Standard Grade Concrete Mix,” Architecture and Civil Engineering, V. 8, No. 1, 2010, pp. 23-34. doi: 10.2298/FUACE1001023K
6. Cusson, D., and Hoogeveen, T., “Internal Curing of High-Performance Concrete with Pre-soaked Fine Lightweight Aggregate for Prevention of Autogenous Shrinkage Cracking,” Cement and Concrete Research, V. 38, No. 6, 2008, pp. 757-765. doi: 10.1016/j.cemconres.2008.02.001
7. Bentz, D. P., and Stutzman, P. E., “Internal Curing and Microstructure of High-Performance Mortars,” Internal Curing of High-Performance Concretes: Laboratory and Field Experiences, SP-256, B. J. Mohr and D. P. Bentz, eds., American Concrete Institute, Farmington Hills, MI, 2008, pp. 81-90.
8. Gifta, C. C.; Prabavathy, S.; and Kumar, G. Y., “Study on Internal Curing of High Performance Concrete Using Super Absorbent Polymers and Lightweight Aggregates,” Asian Journal of Civil Engineering, V. 14, 2013, pp. 773-781.
9. Vedhasakthi, K., and Saravanan, M., “Development of Normal Strength and High Strength Self-Curing Concrete Using Super Absorbing Polymers (SAP) and Comparison of Strength Characteristics,” International Journal of Research in Engineering and Technology, V. 3, No. 10, 2014, pp. 310-316. doi: 10.15623/ijret.2014.0310050
10. Liu, J.; Tang, K.; Qiu, Q.; Pan, D.; Lei, Z.; and Xing, F., “Experimental Investigation on Pore Structure Characterization of Concrete Exposed to Water and Chlorides,” Materials (Basel), V. 7, No. 9, 2014, pp. 6646-6659. doi: 10.3390/ma7096646
11. Bentz, D. P., and Stutzman, P. E., “Curing, Hydration, and Microstructure of Cement Paste,” ACI Materials Journal, V. 103, No. 5, Sept.-Oct. 2006, pp. 348-356.
12. Mindess, S.; Young, J. F.; and Darwin, D., Concrete, second edition, Upper Pearson Education, Inc., Upper Saddle River, NJ, 2003, 644 pp.
13. ASTM C136/C136M-14, “Standard Test Method for Sieve Analysis of Fine and Coarse Aggregates,” ASTM International, West Conshohocken, PA, 2014, 5 pp.
14. ASTM C494/C494M-15a, “Standard Specification for Chemical Admixtures for Concrete,” ASTM International, West Conshohocken, PA, 2015, 10 pp.
15. ASTM C31/C31M-15a, “Standard Practice for Making and Curing Concrete Test Specimens in the Field,” ASTM International, West Conshohocken, PA, 2015, 6 pp.
16. ASTM C1723-10, “Standard Guide for Examination of Hardened Concrete Using Scanning Electron Microscopy,” ASTM International, West Conshohocken, PA, 2010, 9 pp.
17. ASTM E1508-12a, “Standard Guide for Quantitative Analysis by Energy-Dispersive Spectroscopy,” ASTM International, West Conshohocken, PA, 2012, 9 pp.
18. ASTM C39/C39M-15a, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2015, 7 pp.
19. Franus, W.; Panek, R.; and Wdowin, M., “SEM Investigation of Microstructures in Hydration Products of Portland Cement,” 2nd International Multidisciplinary Microscopy and Microanalysis Congress, 2015, pp. 105-12.
20. Gnana Venkatesh, S.; Arun, M.; and Arunachalam, N., “Effects on Concrete Strength by Three Types of Curing Methods,” International Journal of Engineering and Management Research, V. 4, No. 6, 2014, pp. 6-8.
21. Stutzman, P. E., “Scanning Electron Microscopy in Concrete Petrography,” National Institute of Standards and Technology, V. 1, No. 1, 2001, pp. 59-72.
22. Klemm, A., and Sikora, K., “Superabsorbent Polymers in Cementitious Composites,” Construction Materials and Structures, 2012, pp. 57-67.
23. Zhutovsky, S.; Kovler, K.; and Bentur, A., “Influence of Cement Paste Matrix Properties on the Autogenous Curing of High-Performance Concrete,” Cement and Concrete Composites, V. 26, No. 5, 2004, pp. 499-507. doi: 10.1016/S0958-9465(03)00082-9
24. Popovics, S., “Effect of Curing Method and Final Moisture Condition on Compressive Strength of Concrete,” ACI Journal Proceedings, V. 83, No. 4, July-Aug. 1986, pp. 650-657.
25. Raheem, A. A.; Soyingbe, A. A.; and Emenike, A. J., “Effect of Curing Methods on Density and Compressive Strength of Concrete,” International Journal of Applied Science and Technology, V. 3, No. 4, 2013, pp. 55-64.
26. Dayalan, J., and Buellah, M., “Internal Curing of Concrete Using Prewetted Lightweight Aggregates,” International Journal of Innovative Research in Science, Engineering and Technology, V. 3, No. 3, 2014, pp. 1-7.
27. Bentz, D. P., and Weiss, W. J., “Internal Curing: A 2010 State-of-the-Art Review,” NISTIR 7765, U.S. Department of Commerce, Washington, DC, 2011, 82 pp.