Title: Prediction of Concrete Pumping: Part I—Development of New Tribometer for Analysis of Lubricating Layer

Author(s): Seung Hee Kwon, Chan Kyu Park, Jae Hong Jeong, Seon Doo Jo, and Seung Hoon Lee

Publication: Materials Journal

Volume: 110

Issue: 6

Appears on pages(s): 647-656

Keywords: concrete pumping; lubricating layer; prediction; rheological properties; tribometer

DOI: 10.14359/51686332

Date: 11/1/2013

Abstract:
The character of the lubricating layer formed near the wall of a pipe during the flow of pumped concrete is a dominant factor facilitating concrete pumping. To predict flow rates of concrete transported by pumping, it is necessary to measure the rheological properties of the lubricating layer before pumping. In this paper, a new version of a test instrument called a tribometer is developed by considering the level of shear rate that induces the lubricating layer during real pumping. A test method is also suggested based on numerical simulation of the shear flow inside the tribometer and, finally, equations capable of transforming the values measured in the new tribometer into the rheological properties of the lubricating layer are derived. Work in this paper will be extended in a subsequent paper in which full-scale pumping tests will be performed, and predictions for concrete pumping based on the measurements of the new tribometer will be verified from comparisons with the test results.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer