Effect of Ultra-High-Performance Concrete on Pullout Behavior of High-Strength Brass-Coated Straight Steel Fibers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Ultra-High-Performance Concrete on Pullout Behavior of High-Strength Brass-Coated Straight Steel Fibers

Author(s): Kay Wille and Antoine E. Naaman

Publication: Materials Journal

Volume: 110

Issue: 4

Appears on pages(s): 451-462

Keywords: equivalent bond strength; single-fiber pullout; straight fibers; ultra-high-performance concrete (UHPC); ultra-high-performance fiberreinforced concrete (UHP-FRC).

DOI: 10.14359/51685792

Date: 7/1/2013

Abstract:
The objective of this research was to investigate the pullout behavior of straight high-strength steel fibers embedded in different ultra-high- performance concretes (UHPCs) with a compressive strength ranging from 190 to 240 MPa (28 to 35 ksi). Particular attention was placed on obtaining matrixes with high packing density to enhance the physicochemical bond with the embedded fiber. The parameters investigated included the use of different sand ratios, silica fume (SF) and glass powder with different mean particle sizes, different superplasticizers, and the addition of hydrophilic or hydrophobic nanosilica particles. Thus, by tailoring the matrix composition, significantly different bond stress versus slip-hardening behaviors were achieved. This is atypical for straight smooth steel fibers, which are normally characterized by a bond-slip softening behavior. Microscopical studies revealed that scratching and delaminating of the brass-coated fiber surface by fine sand and by abrading matrix particles is one reason for this phenomenon, and help explain the maximum equivalent bond strength observed of up to 20 MPa (2.9 ksi).