slag in concrete Topic

RESULTS FOR SLAG IN CONCRETE

Definition: granulated blast-furnace slag that has been finely ground and that is hydraulic cement.- ACI Concrete Terminology


The use of slag in concrete has several benefits, including reduced energy, reduced greenhouse gas emissions, and reduced use of raw materials. Various types of slag are produced: - Blast-furnace slag—The nonmetallic product, consisting essentially of silicates and aluminosilicates of calcium and of other bases, that is developed in a molten condition simultaneously with iron in a blast furnace. - Air-cooled blast-furnace slag—The material resulting from solidification of molten blast-furnace slag under atmospheric conditions; subsequent cooling may be accelerated by application of water to the solidified surface. - Expanded blast-furnace slag—The lightweight, cellular material obtained by controlled processing of molten blast-furnace slag with water or water and other agents such as steam, compressed air, or both. - Granulated blast-furnace slag (GBFS)—The glassy granular material formed when molten blast-furnace slag is rapidly chilled, as by immersion in water. - Ground-granulated blast-furnace slag (GGBFS)—Now known as cement, slag—granulated blast-furnace slag that has been finely ground and that is a hydraulic cement.


   Informational Resources      News, Events & Engagements      ACI Web Pages   

JOURNAL Articles ON SLAG IN CONCRETE

Multi-response Optimization of Quaternary Blended Mortar Using Taguchi–Grey Relational Analysis

Publication: IJCSM
Date: 3/31/2026

Investigating Pozzolanic Reactivity of Ground Ferronickel Slag Through the R3 Test for Its Potential Use as Alternative Supplementary Cementitious Material

Publication: IJCSM
Date: 3/31/2026

Self-Healing Capability of Ambient Cured High Calcium Based Alkali-Activated Engineered Composites (Prepublished)

Publication: Materials Journal
Date: 3/25/2026

Effects of Different SCM on ASR of Seawater Sea-Sand Cement-Based Materials (Prepublished)

Publication: Materials Journal
Date: 3/25/2026

Optimized Fiber-Reinforced Slag Concrete for Freezing-and-Thawing Resilience

Publication: Materials Journal
Date: 3/1/2026

Surface Treatment for Recycled Plastic Aggregate in Concrete: A Review

Publication: Materials Journal
Date: 3/1/2026

Effects of Limestone Powder on Chloride Concentration of Cement Paste

Publication: Materials Journal
Date: 3/1/2026

Mitigating Chloride-Ion Ingress in Cement Composite Using Nanosilica

Publication: Materials Journal
Date: 3/1/2026

Alkali Silica Reactivity in Cement Composite with Ferronickel Slag Aggregates: A Regression Analysis and 3D Visualisation Approach

Publication: IJCSM
Date: 1/31/2026

Multi-objective Optimisation of One-Part Slag–Flyash–Microsilica Based Alkali-Activated Ternary Binder Mixes

Publication: IJCSM
Date: 1/31/2026

Search all Articles on slag in concrete »

Practice oriented papers and articles ON SLAG IN CONCRETE

2025 Slag Cement in Sustainable Concrete Awards

Publication: Concrete International
Date: 5/1/2026

Potential of grinding agent for enhancing chemical reactivity of blast furnace and steel slag materials

Publication: Special Publication
Date: 5/1/2026

Point of View: Type IL Cement and Concrete Scaling

Publication: Concrete International
Date: 4/1/2026

What’s Next After Type IL Cement and How Can We Use Blended Cements Successfully?

Publication: Concrete International
Date: 2/1/2026

Chloride Desorption Isotherms of Cementitious Systems Exposed to Low-pH Environments

Publication: CRC
Date: 8/5/2025

Point of View: Type IL Cement and Concrete Scaling

Publication: Concrete International
Date: 7/1/2025

2024 Slag Cement in Sustainable Concrete Awards

Publication: Concrete International
Date: 5/1/2025

Study on Use of MSWI Fly Ash with Mainstream Supplementary Cementitious Materials

Publication: Special Publication
Date: 6/18/2024

Efficiency of Using Recycled Coarse Aggregate for Internal Curing of Blended Cement Concretes

Publication: Special Publication
Date: 6/18/2024

Comparative Study of the Mechanical and Durability Performance of Low Carbon Concrete Matrices with Alternative SCMs

Publication: Special Publication
Date: 6/18/2024

Search all Articles on slag in concrete »