Fatigue

Definition: the weakening of a material by repeated loads.- ACI Concrete Terminology


Concrete fatigue refers to the phenomenon of rupture under repeated loadings, each of which is smaller than a single static load that exceeds the strength of the material. Fatigue is exhibited when a material fails under stress applied by direct tension or compression, torsion, bending, or a combination of these actions.

ACI Web Pages


Advanced Tips
Type Example Notes
Fuzzy kettle~ Contain terms that are close to the word kettle, such as cattle
Wild cat* Contain terms that begin with cat, such as category and the extact term cat itself
Exact-Single orange Contain the term orange
Exact-Phrase "dnn is awesome" Contain the exact phase dnn is awesome
OR orange bike Contain the term orange or bike, or both. OR, if used, must be in uppercase
orange OR bike
AND orange AND bike Contain both orange and bike. AND must be in uppercase
Combo (agile OR extreme) AND methodology Contain methodology and must also contain agile and/or extreme
Results Per Page:
select
Limit the search results with the specified tags
Limit the search results modified within the specified time
select
Limit the search results from the specified source
select
Search results must exactly contain the keywords