On-Demand Course: Advancing Durable Foundations: Experimental Performance of GFRP Piles Under Different Loading Conditions

On-Demand Course: Advancing Durable Foundations: Experimental Performance of GFRP Piles Under Different Loading Conditions

Price: $ 39.00 USD

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

INSTRUCTIONS: View the recorded webinar. Complete 10-question quiz with a score of 80% or higher to receive a certificate for 0.10 CEU (equivalent to 1.0 PDH).

Continuing Education Credit: 0.10 CEU (1.0 PDH)

Approved AIA and ICC

Access Period: 30 days

Description

This is a recorded webinar from September 14, 2026.

This webinar is jointly sponsored by NEx: An ACI Center of Excellence for Nonmetallic Building Materials and the American Concrete Institute (ACI).

This webinar presents the key findings from an experimental research programme investigating the performance of glass fiber-reinforced polymer (GFRP) piles under different loading conditions. Using geotechnical centrifuge testing, the project evaluated pile response, load-transfer mechanisms, deformation, strain distribution, and soil–pile interaction at prototype stress levels. The presentation will highlight the testing methodology, instrumentation, data interpretation procedures, and the principal behavioural trends observed across the loading cases. The performance of GFRP piles will be directly compared with that of conventional steel piles to identify similarities, differences, and potential design implications. The webinar will also discuss the practical relevance of GFRP piles for durable foundation systems, particularly in aggressive environments, and will outline the remaining research needs required to support broader engineering implementation.

 

Document Details

Author: Tarek Abdoun

Publication Year: 2026

ISBN:

Categories: Design, Durability, Fiber-Reinforced Polymers(FRP), Testing

Formats: Online Learning

Table of Contents

Learning objectives:

1. Explain the motivation for using GFRP piles and the principal engineering questions addressed by the research programme.

2. Describe the geotechnical centrifuge testing methodology, instrumentation, and data-analysis procedures used to evaluate GFRP pile performance.

3. Interpret the load–displacement response, strain distribution, bending response, and soil–pile interaction observed under different loading conditions.

4. Compare the behaviour of GFRP and conventional steel piles and identify the potential implications for pile design, durability, and future implementation.

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Quantity Discounts

This item qualifies for quantity discounts. Discounts are reflected in the shopping cart.
Quantity Discount
10 - 19 25%
20 - 49 35%
50+ copies 50%