Description

Proceedings of the second ACI sponsored Refractory Concrete Symposium. Ten papers are presented. Topics include advances in refractory concrete technology; problems and solutions in using these materials as liners in coal gasification equipment, aluminum melting and holding, refining and petrochemical operations, and steelmaking; nondestructive testing and evaluation; and repair techniques.

 

Document Details

Publication Year: 2002

Pages: 168.00

ISBN: 9780870317422

Categories: Refractory Concrete

Formats: PDF

Table of Contents

-Recent Advances in Refractory Concrete Technology by Wate T. Bakker

-Castable Refractory Design Requirements by S.A. Bortz, R.F. Firestone, and M.J. Greaves

-Advances in NonDestructive Evaluation Methods for Inspection of Refractory Concretes by William A. Ellingson

-Rational Design with Monolothic Refractories by Timothy J. Fowler

-Analysis and Solution of Refractory Concrete Failure in a Sinter Plant Mist Separator by Richard Shultz

-How to Make Quality Refractories Fail by Wesley C. Lueking

-Performance of Refractory Concretes in Aluminum Heating and Holding Operations by Richard G. LaBar

-Refractory Problems and Repair Techniques in Refining and Petrochemical Operations by M.S. Crowley

-Premature Failures with Monolithic Refractories: The Manufacturer's Viewpoint by Robert E. Fisher

-Repairing Monolithic Refractory Failures by I. Leon Glassgold.

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).